Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vqIVI-0000ajC; Fri, 31 Jan 97 06:55 CST |
Old-Return-Path: |
|
Date: |
Fri, 31 Jan 97 07:48:36 EST |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"HsYtO2.0.KLD.BlUyo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Resent-Sender: |
|
From [log in to unmask] Mon Feb 3 14: |
54:21 1997 |
Message-Id: |
|
Parts/Attachments: |
|
|
Is the 'increased etch speed' that you refer to be due to a galvanic
effect?
MB
______________________________ Reply Separator _________________________________
Subject: Re: Gold as Etch Resist
Author: [log in to unmask] at SMTPLINK-HADCO
Date: 1/30/97 12:48 AM
From my past experience, I have found that when using gold as an etch
resist, the best way to avoid slivers is to run jobs using 1/2 oz base
foil. I was never able to characterize the increase in etch speed to
successfully etch thicker foil. When I got jobs that had a build that
utilized 1 and 2 oz copper foil, we usually ended up with slivers.
______________________________ Reply Separator _________________________________
Subject: Gold as Etch Resist
Author: [log in to unmask] at corp
Date: 1/29/97 3:41 PM
Hello,
Please post information, experiences, and anecdotes, on using
electroplated gold as an etch resist. In particular how is the etch
rate controlled. How can the undercut be reduced to eliminate the
chance of slivers.
(Gold/Nickel/Copper/FR4 :The copper gets etched)
Thanks
Rich
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|