TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charlie Pitarys <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Charlie Pitarys <[log in to unmask]>
Date:
Tue, 4 Mar 2008 15:00:15 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (92 lines)
Why is it wrapped in Crime Scene tape?

Actually it kinda resembles the Chariot from Lost in Space.

;-)

 	


  


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Tuesday, March 04, 2008 9:20 AM
To: [log in to unmask]
Subject: [TN] SV: [TN] NTC Our New Toy

Is it a Mitsubishi Space Wagon or a cableway cabin? 
Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Steve Gregory
Skickat: den 4 mars 2008 14:03
Till: [log in to unmask]
Ämne: [TN] NTC Our New Toy

Good Mornin' All!
 
Well, woke up this morning to a couple inches of snow on the ground.
Winter is hanging on here tenaciously. What's strange, is that it was in
the mid 70's on Sunday!
 
Monday's usually can be pretty blah, but yesterday my Monday was pretty
cool! We got a new toy yesterday:
 
http://stevezeva.homestead.com/files/New_Toy.jpg
 
Got it off the skid yesterday afternoon after spending most of the
morning taking the crate apart. Whoever boxed this thing up had their
nailgun on full-auto! It was quite a job taking the crate apart.
 
Can't wait to get it in place and fire it up. Service engineer will be
in next Monday to do the installation. We still have quite a bit of work
yet. Got to get the old machine moved, and I still have ONE MORE solder
pot to empty. I've pretty much had enough of emptying solder pots. This
will be my third pot in less than two weeks. All-in-all, I'll have moved
over 3,000-lbs. of solder from once place to another, one ladle at a
time.
 
I like new toys, but it's a lot of work!
 
Steve

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2