TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 31 Oct 2003 13:19:52 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
"Jason W. Gregory" <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (72 lines)
Eddie,

I'm not meaning to sound asinine, but I would concerned about reworking
components (especially BGA's) 2 to 3 times regardless of the laminate. Why
the rework?



Jason Gregory
SMT Production Supervisor/
Integrated Product Team Leader
LaBarge Inc.
(918)459-2367
(918)459-2221 fax
[log in to unmask]
http://www.labarge.com






                      Eddie Rocha
                      <[log in to unmask]        To:       [log in to unmask]
                      M>                       cc:
                      Sent by: TechNet         Subject:  [TN] FR4 and rework
                      <[log in to unmask]>


                      10/31/2003 01:37
                      PM
                      Please respond to
                      EddieR






Should there be a concern when reworking BGA's 2 to 3 times when
using 170Tg Fr4? Is there a better choice for the laminate when this
much rework is expected.


-- Thanks,
Eddie Rocha
(408) 978-8992 x 282

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2