TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Roland Jaquet <[log in to unmask]>
Date:
Wed, 7 Jun 2006 15:46:48 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Lee parker <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
Roland

The real issue may be the ability of the test probe to penetrate the surface
being tested. In some past studies we found that the probe pressure and pin
type used on HASL boards was inadequate for OSP and gold/nickel boards. Also
some OSPs present a barrier to the probe that can not be easily overcome
which is why in these cases it is necessary to test the bare board prior to
applying the OSP. If the OSP is not removed in assembly this same barrier
can cause testing difficulties after assembly.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389

----- Original Message -----
From: "Roland Jaquet" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 07, 2006 11:50 AM
Subject: [TN] Electrical test Failures on Bare Board Finsihes, in particular
OSP


> Dear Technetters,
>
> Earlier today I sent an email that for some reason got erased. I
> apologize.
>
> I am wondering if there is some knowledge regarding the surface electrical
> insulation / resistance depending on the type of Surface Finishes such as
> for the bare PCBs as below:
>
> #1 Electroless Nickel Immersion Gold
> #2 Immersion Tin
> #3 HAL Lead free
> Organic Solderability/Surface Preservative
> Electroplated nickel & gold
> Electroless nickel immersion thick gold
> Immersion Silver
> Electroless  Nickel & Palladium, Immersion Gold
> Hot air solder leveling
> Electroless Thick Gold
> SAC
> (any finishes I am missing here?)
>
> For instance, I am wondering what could be the resistance of an OSP finish
> if the contact is such as a feather and flat, versus conical point digging
> in?
>
> Anyone met this kind of problem yet?
>
> In our case, we are considering contact less Electrical Test and we worry
> about the different issues we could get in with such a process!
>
> Any suggestion?
>
> Thank you
> Best Regards
> Roland
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2