Actually, Polyclad does have a material that meets this spec. It is PCL 370
Tetrafunctional resin with a tg of 170oC.

Contact Polyclad on 603 934 5642

Best regards,

Colin William

At 14:21 04/03/99 -0500, you wrote:
>IPC-4101 references a laminate material IPC-4101 /26 that has a minimum tg of
>170 degrees C. PolyClad does not make a match for this material does
anyone know
>of a laminate manufacturer that does?
>
>Thanks,
>Dave Kumpf
>L-3 Communications-East
>Camden, NJ
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2