Dan,
good plating shall not be able to remove it easily, slightly remove the
surface layer normally is good for wire bonding.  what kind of plating
surface you use?
                                                      jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Dan R. Johnson
>Sent: Wednesday, September 25, 2002 11:57 AM
>To: [log in to unmask]
>Subject: Re: [TN] How to use gold finished boards that have been
>handled?
>
>
>*Caution* use a "Pink Pearl" type eraser, the type used for ink will remove
>the gold plate. (He remarked sheepishly.) Yes, this is the voice of
>experience. I learned this lesson in the eighties
>building/repairing traffic
>controller modules.
>Dan
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2