TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steven Creswick <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Date:
Wed, 5 Feb 2014 20:47:46 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (80 lines)
Wayne,

Amen!

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Wednesday, February 05, 2014 7:44 PM
To: [log in to unmask]
Subject: Re: [TN] Wire Bonding Spec?

I don't want to get in some kind of on line spat over this, but I recommend
that whoever is doing the wirebonding calls out the surface finish!  If that
person has any experience, they will only commit to the finish after the
vendor provides a sample they can test with.  For many this would not be
enough and they would send it out to a lab for full analysis so they can use
it as a baseline and verify that the actual production boards have the same
finish.

Wirebonding issues mostly have to do with surface finish and contamination:
Solve those and generally you can have a pretty good day!

Wayne Thayer

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth Wood
Sent: Wednesday, February 05, 2014 6:51 PM
To: [log in to unmask]
Subject: Re: [TN] Wire Bonding Spec?

Jack,
Use ENEPIG surface finish. A bit pricey but pretty good for wire bonding.
Ken
_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.              
[log in to unmask]
(407) 340-2668
www.saturnpcb.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Wednesday, January 29, 2014 4:17 PM
To: [log in to unmask]
Subject: [TN] Wire Bonding Spec?

newbie question:

Do any IPC publications discuss wire bonding?
What we are trying to do is similar to COB, but this is a new subject for
us...

thanks,
Jack


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2