Time and money. You can place a lot of glue dots onto a board in a
matter of 20 seconds or less with a stencil and a cheap screen printer.
Of course, you reach a point of diminishing returns when only a handful
of glue dots are needed. I tend to think of glue stencils as "old
school" since selective wave solder pallets have been around for ages...
Ryan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of legg
Sent: Wednesday, June 18, 2008 9:42 AM
To: [log in to unmask]
Subject: Re: [TN] Glue Mask Requirements
Don't mean to side-track this thread, however this is the first time
I've seen a reference to glue or epoxy masking.
My work has used spot adhesive despensing techniques for wave-
side and some other smd for some years on mixed technology power
assemblies. This is not always specifically for retention purposes.
I'd have difficulty transferring knowledge accumulated using this
method to masking. The very idea sounds incredibly messy - I'd
even be tempted to use disposable stencils.
Any good references or reasons why masking is preferable?
Rob Legg
Power Electronics Specialists
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|