I have a question for the assembly folks out there;
We just recieved notification that one of our connectors
is no longer available with tin/lead plating contacts,
and that they are now tin/bismuth.
I searched the last two years of Technet archives for
the word "bismuth" and only found this one comment with
no other responses:
(there were other posts with "bismuth", but not relevant)
-=-=-
Some component lead-free finishes are not compatible with
current tin/lead assembly processing. Bismuth can weaken
tin-lead solder joints. Tin finishes should only be matte
(no brighteners) or fully annealed (low stress to ensure
against tin whiskers that can ruin satellites and cause
fires).
Karl Sauter
Staff Engineer, Engineering Technologies
Sun Microsystems Inc.
-=-=-
We are NOT using a lead-free assembly process.
Someone PLEASE give me some good news....
Jack
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------