TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Karnwal, Pankaj" <[log in to unmask]>
Date:
Mon, 27 Jan 2003 07:55:52 +0100
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Karnwal, Pankaj" <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Hi All
 Further my Question  "IS the Oval shape pads on PCB for BGA  soldering
help for better analysis in x-ray inspection". We are using that type of
pads in our prod. and when we see the  round image of any  ball we assume
that this ball is not soldered properly and the solder flow is less so we do
rework for the same. Is that the correct method?
your opinion Pls.
Thanks
With regards
Pankaj Karnwal
QualityAssurance
BESL A-4,Sec-5 NOIDA,201301,INDIA
e mail : <mailto:[log in to unmask]>
Barco,innovators in image processing


> ----Original Message-----
> From: Werner Engelmaier [SMTP:[log in to unmask]]
> Sent: Monday, January 27, 2003 6:07 AM
> Subject:      Re: BGA micro cracks
>
> Hi David,
> When you get intermittents, that means you have a full crack not a
> micro-crack. Fractured solder joints are notorious for this, and cannot be
> found by X-ray or visual innspection. Your description makes me suspect
> not
> so much solder joint cracking, but interfacial separation due to 'black
> pad'
> or a similar problem causing an absence of a metallurgical bond.
> Cross-section some of these joints to see what you have, an effective
> screening procedure is vibration.
>
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL  32174  USA
> Phone: 904-437-8747, Fax: 904-437-8737
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2