We still use local ficucials for all of our fine pitch parts, but then
again, we're using fairly old placement equipment. Our Panasonic MPA
flexible placer is over 5 years old...

At 11:20 AM 6/5/98 -0500, you wrote:
>Hello everyone,
>
>I am trying to find out if anyone is still requiring local fidutials on fine
>pitch patterns.
>
>Does anyone REALLY use them?
>
>They  consume a lot of real estate.  Todays placement machines do an
>excellent job using only the global fidutials.
>
>Your responses are greatly appreciated !
>
>
>Russ Vertefeuille
>Sr. Project Eng.
>Honeywell, BCAS
>Glendale, AZ
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
----

Jeffrey C. Guynn <[log in to unmask]> Phone: (219) 429-6345
Lead SMD Manufacturing Engineer        Fax: (219) 429-4688
Raytheon Systems Company M/S 25-31
1010 Production Road, Fort Wayne, IN 46808-4106

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2