TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Fri, 11 Jun 2010 15:37:15 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
<6AF520ECAE2FD611BF8E00C09F065566021DFE70@server>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (287 lines)
Hi Kenny - there was an excellent article on the calculator in the 
American Scientific Journal during the last 6-7 months which is also a 
very good read for the science minded. The sleuthing of how the number of 
gear teeth interact and rotate to produce the ancient calendar events was 
a very interesting math and mechanical engineering exercise. Modern 
engineering isn't as advanced as we sometimes want to believe.

Dave



Ken Bloomquist <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
06/11/2010 03:17 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ken Bloomquist <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] NTC:Friday quiz 8






It's an astronomical calculator from around 100 BC. It was used to predict
the locations of the planets, moon phases, eclipse and more. It was way
ahead of it's time with some of the technology not being developed until 
the
18th Centruy!

Google it, very cool!

KennyB

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, June 11, 2010 12:57 PM
To: [log in to unmask]
Subject: Re: [TN] NTC:Friday quiz 8

I think one can't come closer. Ken is the winner.  But the 'talented' is 
the

one who can figure out what it really is, because noone knows today.  A 
clock? Hardly 1,000 years B.C.  Personally, I believe it's some kind of a 
symbolic  gem for worshipping a goddess.  We think too much in terms of 
machinery, scientists and engineers as we are.
Inge

--------------------------------------------------
From: "Ken Bloomquist" <[log in to unmask]>
Sent: den 11 June 2010 20:00
To: <[log in to unmask]>
Subject: Re: [TN] NTC:Friday quiz 8

> Antikythera Mechanism
>
> KennyB
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Friday, June 11, 2010 11:04 AM
> To: [log in to unmask]
> Subject: Re: [TN] NTC:Friday quiz 8
>
> Here it is:
>
> http://stevezeva.homestead.com/Friday_Quiz_8.jpg
>
> Steve
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
> Sent: Friday, June 11, 2010 1:01 PM
> To: [log in to unmask]
> Subject: Re: [TN] NTC:Friday quiz 8
>
> Drew, You have the chance to make it this week.  Depends on what Steve
> decides.
> The one who can guess this correctly is very talented.
> /Inge
>
> --------------------------------------------------
> From: "Inge" <[log in to unmask]>
> Sent: den 28 May 2010 21:19
> To: "Drew meyer" <[log in to unmask]>; <[log in to unmask]>
> Subject: Re: NTC:Friday quiz 7
>
>> Drew,
>> Not at all.  Based on your touching story,  your (nowadays rare) good
>> representation of american open minded way of sharing a family 
experience
>> with us all, I decide that Wendy and you are both winners.  But next
>> week's quiz will be level III .  You will spit out your Wrigley and
>> scratch your blackbird colored  skull.
>> Have fun.  And make TN even better.
>> /Inge
>>
>>
>>
>> --------------------------------------------------
>> From: "Drew meyer" <[log in to unmask]>
>> Sent: den 28 May 2010 19:18
>> To: <[log in to unmask]>; "Ingemar Hernefjord" <[log in to unmask]>
>> Subject: Re: NTC:Friday quiz 7
>>
>>> Inge,
>>>
>>> I must admit that due to my birth date and historical condtions I have
>>> not
>>> been in the service.  My father was drafted in WWII.
>>>
>>> My exposure to the machine was at large town nearby on the 4th of 
July.
>>> Every year the Army Reserve/National Guard sets up a display manned by
>>> volunteers.  Some gear is there and you can sit in a military Hummer 
and
>>> see
>>> other things.
>>>
>>> One year they had the Dog Tag machine and if you waited in line a long
>>> time
>>> on a very hot day they would make you a Dog Tag.  My wife gave up but 
I
>>> stuck it out just to see it work.  There were a few dud tags tossed 
that
>>> day.
>>> In the end I had a dog tag made for"""""""""""".  My wife's dog!  Very
>>> friendly
>>> and prone to wander (sneak away) if not watched closely.  The few 
times
>>> CoCo (Yorkie Poodle mix) snuck away the tag hit pay dirt.  Where ever 
he
>>> ended up in town we received a phone call and went to get him.
>>>
>>> He passed away with my wife holding him at the Vet.  He was 17 and 
life
>>> was
>>> very hard for him.  He was blind, deaf and incontinent by then.
>>>
>>>    My wife still has the tag.
>>>
>>> Based on your response I have missed the mark too.
>>>
>>> Drew
>>>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16

> for additional information, or contact Keach Sasamori at [log in to unmask] 
or

> 847-615-7100 ext.2815
> ----------------------------------------------------- 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2