TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w4Wnd-000BBhC; Tue, 11 Mar 97 13:01 CST
From [log in to unmask] Tue Mar 11 15:
14:41 1997
Old-Return-Path:
Date:
Tue, 11 Mar 97 11:08:42 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11028
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"XZWom3.0.Lc9.4mQ9p"@ipc>
Subject:
From:
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (38 lines)
     We use HASL at this time.
     
     -msa


______________________________ Reply Separator _________________________________
Subject: FAB: ALTERNATIVE TO HASL
Author:  [log in to unmask] at _internetcc
Date:    3/11/97 7:13 AM


I'd like to do a small survey.
What is the most accepted alternative to hot air leveling? 
Why?
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2