TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 15 Aug 2008 07:16:05 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (109 lines)
Do you have the product P/N?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Friday, August 15, 2008 1:14 AM
To: [log in to unmask]
Subject: Re: [TN] Yellow Colored Visible Dye Penetrant

In the UK the material is available from Ely Chemical:

It has a UV trace but I always use red with my customers as its easier
to
see on the surface of samples.

Ely Chemical Co Ltd
Lisle Lane
Ely
Cambridgeshire
CB7 4AS
Tel:  +44 (0)1353 665881
Fax:  +44 (0)1353 664623
Web: www.elychemical.com
Email: [log in to unmask]


Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 3rd
September www.ASKbobwillis.com/PCBworkshop.pdf 
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 11th
September  www.ASKbobwillis.com/faworkshops.pdf
 
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of bob wettermann
Sent: 14 August 2008 22:33
To: [log in to unmask]
Subject: [TN] Yellow Colored Visible Dye Penetrant

Dear Technetters:

Has anyone purchased yellow visible colored dye penetrant for dye and
pry
testing? Can someone recommend a vendor?

BTW this was recommend to me by an end user in japan as some copper
problems
are "hidden" by the typical red visible dye penetrant.

Thanks

Bob Wettermann


Bob Wettermann
PH 847-767-5745

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2