Tom,
This issue was diss in the forum. Since board can not be
rotated, rotate TO-92 pkg as shown.
1. Direction thru wave ------------------->
O O
O or O
O O
OR you could add a robbing pad as shown
2. Direction thru wave ------------------->
O O O
O
I am using Kester 951 as you do, I have no problem with the first
option layout. My pad layout is smaller than the one
you mentioned with a small section cut-out on the side of two
pads facing each other as shown.
CI D
O
regards
Matthew Park
Norsat International Inc.
>>> "Fawn Industries, Elm City Plant"
<[log in to unmask]> January 6, 1999 10:42 am
>>>
Techies,
I have a PCB that uses 30-40 T0-92 transistors. My problem is
that when I
wave solder these PCB's, the majority of them have solder
bridges. I
believe the pad-pad spacing ( 0.5mm) is the problem. Lead
protrusion is
1mm, pad size 1.4mm.
Direction thru wave ------------------->
O O
O
Soldering 200-210F until 490F at wave -Tried temp increase
Conveyor speed 4.2ft/min - Tried faster and Slower
Cannot rotate PCB
Have to use NOclean flux - Kester 951
I would like to know what is usually recommended or what some
of you use at
your companies. Any help would be greatly appreciated.
Tom B.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line
Services" section for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|