TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Crawford <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Crawford <[log in to unmask]>
Date:
Wed, 11 Jul 2007 17:22:47 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (129 lines)
Time for the document liaison to comment on this.

The inside cover of every IPC document has these words:
It is the position of IPC's Technical Activities Executive Committee
that the use and implementation of IPC publications is voluntary and is
part of a relationship entered into by customer and supplier.

The statement in Clause 1.9 of J-STD-001 means that someone cannot apply
J-STD-001 to an assembly that has already been built, such as COTS. It's
too late--it would have had to be required for that assembly before it
was built. It doesn't mean that J-STD-001 can't be called out for
building COTS during the procurement process--ultimately that's an
agreement between the customer and the supplier.

To your specific question, regardless whether or not the end product
will be COTS, if 610 is the required assembly acceptance standard and
the standard doesn't have coverage for the specialized (or new)
technology in the assembly, Clause 1.3 states that Class 2 "should" have
customer involvement and Class 3 "needs to have" customer involvement.
COTS is most commonly considered Class 1 or 2, but sometimes COTS gets
used in Class 3 environments.

The problem is that the consumer buying COTS products will never know
what, if any, standard or norm was used to manufacture or accept the
product. Only the manufacturer will know that. I can assure you that
many COTS items are built to IPC-A-610 and some even to J-STD-001. 

Jack

Jack Crawford, IOM
IPC Director Certification and Assembly Technology
[log in to unmask]
847-597-2893
FAX  847-615-5693
3000 Lakeside Drive, Suite 309 S
Bannockburn, IL, 60015

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg A. Owens
Sent: Wednesday, July 11, 2007 10:06 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-610D Section 1.3 Customer Consent

Rob:

Thinking about it, IPC-A-610 Does not specifically address COTS, however
its process cousin does with J-STD-001D which specifically states COTS
are NOT to be covered by J-STD-001. 

1.9 Requirement Flowdown
When this standard is contractually required, the applicable
reuqirements of this standards (including product class) shall be
imposed on all subcontracts, assembly drawings, documentation and
purchase orders. Unless otherwise specified the requirements of this
standard are not imposed on the procurement of commercial-off-the-shelf
(COTS or catalog) assemblies or subassemblies.

Gregg Owens, MIT
Manufacturing Technology Training Center ,Inc.
Mira Loma, CA 91752

-----Original Message-----
>From: Rob Carrillo <[log in to unmask]>
>Sent: Jul 11, 2007 5:24 AM
>To: [log in to unmask]
>Subject: [TN] IPC-610D Section 1.3 Customer Consent
>
>Section 1.3 talks about customer consent for unique definitions of 
>specialized characteristics. Is customer consent required for COTS 
>products?
>
>Regards,
>Rob Carrillo
>Quality Assurance Manager
>North Atlantic Industries
>110 Wilbur Place
>Bohemia, NY 11716
>Tel #: (631) 567-1100 x163
>Fax #: (631) 218-1290
>Direct: (631) 218-1263
>An ISO 9001:2000 Registered Company
>
>
>This message and any attachments are intended only for the use of the
addressee and may contain information that is privileged and
confidential. If the reader of the message is not the intended recipient
or an authorized representative of the intended recipient, you are
hereby notified that any dissemination of this communication is strictly
prohibited. If you have received this communication in error, please
notify us immediately by e-mail and delete the message and any
attachments from your system.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
>unsubscribe, send a message to [log in to unmask] with following text in 
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
>or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
>archives of previous posts at: http://listserv.ipc.org/archives Please 
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

>additional information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2