I remember Colin Thwaites's paper very well and Brian's, was grateful for
them, but no longer have copies. 
I would be surprised if the ITRI people don't find a copy. I asked them for
an actual reference to some information of the industry legend type -
meaning everyone knows it but not why or how they know it - and they found
first references in early 1940s. 

Regards
 
 
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Friday, February 06, 2009 7:30 AM
To: [log in to unmask]
Subject: Re: [TN] In Search of a Technical Reference

Dave

I hadn't realised that Colin Thwaites had published such a paper. I
believe that his research of the subject may have been instigated by
myself, following publication of the paper I presented at Inter/Nepcon
'69, in Brighton, England, 'New Aspects on the Solderability of Printed
Circuits'. Unfortunately, I no longer have a copy of the Technical
Proceedings but, as I remember it (40 years is a long time ago!!!), I
evoked the problems caused by both pumice and ScotchBrite cleaning,
whereby the abrasive particles were embedded into the copper pore
structure and then the copper was swaged over them. The only way they
could be released was with a light persulfate etch and forceful rinse,
without which dewetting was inevitable after abrasive cleaning.

Having written this, I then re-read what I wrote in Section 7.2.4 (p.
76) of my book and found that it's similar in essence but more complete,
so my aged memory can't be that bad! Whatever, abrasives and
solderability make poor bedmates!

Hope this helps.

Brian

David D. Hillman wrote:
> Hi gang! Ok, I am in search of a technical reference and my usual, "always

> works" sources have failed me. I am looking for the following technical 
> reference:
> 
> Thwaites, C. J. and Mackay, C. A. , " Some Effects of Abrasive Cleaning on

> the Solderability of Printed Circuits", Metal Finishing Journal, Sept. 
> 1968, pp. 291-294, (also may be listed as ITRI Publication 386)
> 
> 
> Anyone have a copy or can direct me to where a copy can be obtained? And 
> yes, I have sent a request to the ITRI folks already (International Tin 
> Research Institute)
> 
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2