TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Fri, 11 Apr 1997 17:53:30 -0700
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11917
X-Sender:
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"XacOF.0.UZ7.R6kJp"@ipc>
Subject:
From [log in to unmask] Mon Apr 14 10:
32:14 1997
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wFrNU-000BjcC; Fri, 11 Apr 97 20:13 CDT
From:
Phil Bavaro <[log in to unmask]>
Message-Id:
<v03007802af74259583d7@[129.46.191.125]>
Parts/Attachments:
text/plain (36 lines)
I've been stumped by a phrase which one of our Japanese customers used in a
correspondence with us recently.  The phrase is "Kirkendall void" and the
context it was used in is:

"There are some electrode that are gold plated and also solder welded.  If
there is gold at solder welded part, Kirkendall void may be formedm
resulting pealing."


It is possible that the CCA they were looking at has gold plated leads
installed on gold plated PWBs and reflowed with Sn63Pb37 solderpaste.

Any help would be gratefully accepted,


Regards,


Phillip A. Bavaro
Senior Manufacturing Engineer
[log in to unmask]
(619) 658-2542


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2