Hi, Rick,

I've recommended Eccobond 45 to a number of people for securing components
to substrates for use in hostile environments. In my last company it was
used in military radars where 15g accecerations and very high vibration
levels were breaking not-a-few component leads. The Eccobond proved to be a
successful solution. Don't know about lead times or MOQ's though.

Peter




                    Rick Thompson
                    <rthompson@VENTURAELECTR        To:     [log in to unmask]
                    ONICS.COM>                      cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by: TechNet                Aero/ST Group)
                    <[log in to unmask]>               Subject:     [TN] Adhesive Recommendations?


                    02/13/02 06:14 AM
                    Please respond to
                    "TechNet E-Mail Forum.";
                    Please respond to Rick
                    Thompson






We have an application where we need to secure some vertically mounted
radial electrolytic caps and a few other higher profile items to make
them resistant to shock, impact and vibration (amusement park
application).  I've contacted Loctite and 3M for recommendations but the
ones I've gotten have several week lead times, minimum buys due to
special order, etc. Since we don't know if the products will work, we
didn't want to buy minimum quantities of materials we can't return.

Does anyone have any recommendations for standard products you may have
used in similar situations?  I realize I can get samples from the mfgs.
Noted but I was hoping to shorten the lead time if I can find off the
shelf products that may do the job.

Thanks for your inputs.


Rick Thompson
Ventura Electronics Assembly
2655 Park Center Dr.
Simi Valley, CA 93065

+1 (805) 584-9858   x-304  voice
+1 (805) 584-1529 fax
[log in to unmask]

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2