TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charles McMahon <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 5 Dec 2001 12:33:26 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
EARL:

Does your view hold the same from an assemblers point of view.

More specifically, in your history, would the assembler prefer ENIG over
SILVER and/or TIN?
THe assemblers I speak with just do not have the background/experience to
decide. However, they
are quick to reject the bare board vendor for what they THINK is a
solderability problem.
(That's when I move with failure review etc. I hope to reduce this incidence
dramatically by proposing user friendly finishes based on board design.)

Charlie

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Earl Moon
Sent: Wednesday, December 05, 2001 12:14 PM
To: [log in to unmask]
Subject: Re: [TN] SURFACE FINISHES


As a cost factor to you it's nickle and dime stuff. To most board shops I
work with, it is as well. It's a matter of choice so much that it's almost
subjective (whatever looks best though black pad isn't too pretty) -
excluding HASL, or course. I hope you are right about its final demise.

MoonMann

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2