TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 6 Mar 2013 14:29:14 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (86 lines)
THF brings a tear to my eye. I used it all the time and it never bothered me- it never bothered me- never bothered me - bothered me.
I was doing hydrogenation and polymerizations runs and the building next to our lab made THF. It blew up one day and a half a block of Mogador doesn't exist anymore.
Still great stuff, but I agree with Doug. There are much safer and easier ways to do this.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, March 06, 2013 7:05 AM
To: [log in to unmask]
Subject: Re: [TN] Coating stripping facility

While I agree with Patrick that this stuff works, it is Tetrahydrofuran, a nasty material and very aggressive.  And if you have the possibility of operators mixing soldering irons with THF, you get some frightening breakdown products.  We used to use these, but got away from it completely.

Straight toluene or xylene will strip 1B31 pretty effectively and is much less costly or hazardous than THF, especially if you are doing a few hundred assemblies.  And you have some good recommendations for companies that will do this for you.

Doug Pauls



From:   "Goodyear, Patrick" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   03/06/2013 07:00 AM
Subject:        Re: [TN] Coating stripping facility
Sent by:        TechNet <[log in to unmask]>



Ioan, 

When we need to remove conformal coatings for repairs we use Conformal Coating Remover from Trace Technologies, we get it from TechSpray in Amarillo Texas 806-3728523  www.techspray.com
MSDS (Material Safety Data Sheets) can be found online.    Very effective 
for removing HumiSeal and others. 
We have it in 1Qt. Bulk and in 12.5ml pens, great for spot application. 

Pat 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Tuesday, March 05, 2013 12:19 PM
To: [log in to unmask]
Subject: [TN] Coating stripping facility

Dear Technos,

I'm looking for a facility able to strip 1B31 from a few hundreds of boards preferably in Eastern Canada or US New England. On or offline answers appreciated, no sub contractor is a priori disqualified, even if in CA.

Thanks,

Ioan Tempea, ing.
Ingénieur principal de fabrication / Senior Manufacturing Engineer [signature002]<http://www.digico.cc/>

950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
T+ 1 (450) 967-7100, EXT244
------------------------------------------------------------------------
  [signature001] <http://www.facebook.com/pages/Digico/277076778479>
------------------------------------------------------------------------
Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
Entreprise manufacturière / Gestion du capital humain


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit 
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2