The gold over nickel will be better by far... Oxidation of the
tin/lead will be much greater than you will see on any gold surface.
Our experiments with these showed the greatest difference in a
temperature and humidity environment for a length of time.
Steve O'Hara
HP
______________________________ Reply Separator _________________________________
Subject: [TN] corrosivity HASL v GOLD
Author: Non-HP-evanj ([log in to unmask]) at HP-Vancouver,mimegw10
Date: 2/26/98 9:18 PM
One of our Engineers has asked me to pass on a question. How does the corrosion
resistance of Electroless gold over Nickel (gold thickness of around 7
microinch) compare to horizontal HASL? The target environment is a marine type
environment (salt spray). The customer does not wish to conformally coat the
end product. If anyone has any experience or data in this area I would be most
grateful.
Regards Evan
Evan Jones
Manufacturing Engineer
Bluegum Technology
Ph 61 3 5720 2539 Fax 61 3 5720 2412
Email [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional inform
ation.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
00 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|