TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
Date:
Tue, 18 Aug 1998 18:11:45 +0000
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Melanie Racuya" <[log in to unmask]>
Subject:
From:
Melanie Racuya <[log in to unmask]>
Content-Transfer-Encoding:
7BIT
Sender:
Comments:
Authenticated sender is <mracuya@[192.1.1.215]>
Parts/Attachments:
text/plain (40 lines)
Hello technetters,
        I've been browsing the internet for ipc's standard regarding the
standards that we are to follow regarding the dust particle count.
For a 10K class clean room and a 0.5 microns  particle size, we are
allowed a 10,000 particles  per cu ft.
        In my case, since we are encountering problems regarding fibers and
we have checked that the environment contributes to this problem, we
decided to check the particle count in our area. Using the clean room
standard we failed. What I want to know is : What is the standard
particle count for a particle size of 2 microns? Our environment is
not a clean room environment and we're producing the flex for HDD.
Please help me with this problem...I just need the standard.

Thanks and best regards,

Bing

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2