TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Charles Barker <[log in to unmask]>
Date:
Wed, 12 Nov 1997 13:26:46 -0600
Content-type:
multipart/mixed; Boundary="0__=2mm7OL23vq8JUy1DEeNoMqSuHgWDGhQe4Bq082iBNaTqKC54NFHxTzlY"
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (756 bytes) , att1.unk (1357 bytes)




Charles Barker@IO-US
11/12/97 01:26 PM

Hi Karla,

A few questions for more info:
1. Do you have any input about the pad sizes? For best results, the
wave-soldered pads need to be larger that what is needed for normal paste
and reflow.
2. What is your conveyor speed?
3. What is your solder pot temperature?
4. What is the the orientation of the long side of the SOT23's relative to
the direction of travel thru the wave? What works best is if they are
parallel to the direction of travel.
5. What kind of flux are you using and how is it being applied?
6. Are the SOT23 parts old? Are they solderable in the first place?