TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Tom Moore <[log in to unmask]>
Date:
Mon, 9 Jan 2006 15:51:11 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tom Moore <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
Technetters,
Need your help with an acceptance criteria issue.

Have a SMT board that requires Class 3 acceptance criteria. It has some
FETs with what Figure 7-16 in J-STD -001 calls "Bottom Thermal Plane
Termination" (TO-263s. We are using a heat sink that looks like spider with
the middle section flattened that rests on top of the FET (D2 PAK).
Although the tin/lead pad of the board matches where the heatsink or FET
contact the pad, the screen stencil limits the paste application to
individual dots to prevent the components from floating. The heat sink
manufacturer states that only 50 to 75% of the heat sink needs to contact
the PCB pad for effective thermal conductivity.

The problem is that after reflow no solder is visible on the body or legs
of the heatsink. My inspector is trained to go by Section 5 of 610D which
states that it applies to "soldered connections of all types". However a
bond is definitely there because the heatsink holds even when tugged or
twisted. Is this "good enough" to assure a good thermal and mechanical
connection?

Thank you for your guidance.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2