        A measuring tool that we have found is:

        Accuscore
        Score Depth Measurement Guage
        
        Part No.  547-520

        US Phone number:

        (215) 830-9826



        Wayne Haskins
        PC World

        



______________________________ Reply Separator _________________________________
Subject: FWD>FAB- MEASURING DEVICE F
Author:  [log in to unmask] at INET
Date:    5/3/96 12:23 PM


Mail*Link(r) SMTP               FWD>FAB: MEASURING DEVICE FOR V-CUT
     
Roland-
     
Some "screw thread" micrometers have conical pointed anvil and spindle faces.
     
Another way is to modify a "blade" micrometer, the blades generally are about 
0.7 mm thick by 6 mm wide, and are generally used to measure narrow grooves and 
key-ways.  Most blade micrometers have a nonrotating spindle.  Careful 
modification of the "blade" by precision bevel grinding the width of the blade 
will allow you to form a small radius or flat surface like a "dull-knife blade 
or screwdriver".  A small radius or flat blade anvil allows you to use gauge 
blocks for reference calibrations.  If you form the anvils into knife edges, 
you must use optical calibraton so as not to damage the anvil edges.  You also 
must be careful on torquing the spindle as a knive edge could cut into/through 
the "V" groove.    A small radius or flat anvil lets you measure very close to 
the bottom of the groove, and if you know the groove angle, you can develop a 
conversion table for depth.  Most blade micrometers I'm familiar with only have 
a 25 or 50 mm throat, so they are limited in reach, not to say though a "deep" 
throat micrometer couldn't be modified.
     
Ralph Hersey
[log in to unmask]
     
-------------------------------------- 
Date: 5/3/96 2:59 AM
From: Roland Jaquet
Does anybody knows / sales a micrometer with two facing V's
in order to check the remaining core after a V-cut / scoring ?
     
Where can i find a standard for it ?
     
It seems that not only the remaining core is important, but
also the sharpness of the cut. If the edge of the cut is rounded 
it is much more difficult to depanelize...
     
Thank you, Roland
Roland Jaquet         Technical Director 
Henri Jaquet SA       PCB manufacturer
Geneva Switzerland    Prototypes and small qties 
tel. xx41-22-794-7878 fx. xx41-22-794-3052 
[log in to unmask]
     
     
------------------ RFC822 Header Follows ------------------ 
Received: by quickmail.llnl.gov with SMTP;3 May 1996 02:57:46 -0700
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
  id EAA07229; Fri, 3 May 1996 04:50:17 -0700
Resent-Date: Fri, 3 May 1996 04:50:17 -0700 
Received: by ipc.org (Smail3.1.28.1 #2)
 id m0uFH7z-0000C8C; Fri, 3 May 96 04:26 CDT
Resent-Sender: [log in to unmask] 
Old-Return-Path: <[log in to unmask]>
Date: Fri, 3 May 1996 11:30:21 +0200
Message-Id: <[log in to unmask]> 
X-Sender: [log in to unmask] (Unverified) 
X-Mailer: Windows Eudora Version 1.4.4 
Mime-Version: 1.0
Content-Type: text/plain; charset="us-ascii" 
To: [log in to unmask]
From: [log in to unmask] (Roland Jaquet) 
Subject: FAB: MEASURING DEVICE FOR V-CUT 
Resent-Message-ID: <"5JoGu1.0.qG7.o4TYn"@ipc> 
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/3807 
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
     
     
     



ATOM RSS1 RSS2