David -
AlliedSignal provides Resin Coated Copper with several varying resin
thicknesses with the thinnest being 2 mils. Ranges are 2 mils up to 4
mils. It is available on 18 or 12 micron ml or mls copper foil.
Kevin R. Thomas
MicroVia Materials Product Manager
AlliedSignal Laminate Systems
608.791.2288
----------
>>>From: David Arivett
>>>To: [log in to unmask]
>>>Subject: FAB:Laser vias
>>>Date: Saturday, February 15, 1997 12:54PM
>>>
>>>
>>>
>>>
>>> An article in the February edition of PCFAB talks about laser drilled
>>>micro-vias. It shows a multi-layer stack-up of two cores with pre preg in
>>>the center. The outer layers are formed with resin coated foil. My question
>>>is: how thick is the resin on the foil? I am sure it must be at least 2
>>>mils
>>>in order to have enough resin to encapsulate the inner layer circuitry.
>>>What
>>>is the maximum it might be?
>>>
>>>David Arivett
>>>Cuplex Inc.
>>>
>>>***************************************************************************
>>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>>***************************************************************************
>>>* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
>>>* with <subject: subscribe/unsubscribe> and no text in the body. *
>>>***************************************************************************
>>>* If you are having a problem with the IPC TechNet forum please contact *
>>>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
>>>***************************************************************************
>>>
>>>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|