Thomas,
We recycle the solder paste to the same vendor that takes our dross from the
solder wave. I don't know if all vendors would do the same, but it may be
worth a try!
Good luck.
Richard Hamilton
Clemar Mfg. / Rain Bird
[log in to unmask]
> -----Original Message-----
> From: Thomas Han [SMTP:[log in to unmask]]
> Sent: Wednesday, July 28, 1999 2:29 PM
> To: [log in to unmask]
> Subject: [TN] Solderpaste Recycling
>
> Hi all,
>
> I need to dispose of some old solderpaste, but no one seems to want them
> or
> offer the servoce. I called Kester(my manufacturer), but they'll only
> sell
> you the stuff and do not want anything to do with disposing of them. How
> are you disposing the old solderpaste?
>
> Tom
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|