     Hello Jim -
     
     Alloy Sn46/Pb46/Bi8?? Tough one - the only place I found that alloy 
     mentioned was in JSTD-006. I'll see if I can find you a Sn/Pb/Bi 
     ternary diagram that has the liquidus and solidus points. You might 
     try giving Dave Torp at Kester (847-390-9338, Bill Hampshire 
     (614-841-0835 or Norb Socolowski (201-627-5179) a call - they might be 
     able to help. The discrepancies in the temperature range maybe due to 
     other small alloy additions that the users are not telling you about.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     


______________________________ Reply Separator _________________________________
Subject: ASSY: SOLDER ALLOY MELTING POINT
Author:  [log in to unmask] at ccmgw1
Date:    5/2/97 2:37 PM


I'm trying to find data on the melting point (range) of a particular solder 
alloy, Sn46 Pb46 Bi8.  So far, the temperature ranges I came across are:
     
 120 C to 167 C (IPC-J-STD-006)
     
 163 C to 178 C (a Japanese company)
     
 171 C to 186 C (a component foundry using this alloy - BGAs)
     
As you can see, I have conflicting stories.  Can anyone tell me where I can get 
good information?  (By the way, I don't have a sample to test so don't suggest 
it!)
     
Thanks again,
     
Jim Marsico
(516) 595-5879
[log in to unmask]
     
                        ********************************
                        *       ______   _   _  _____  *
                        *      / ___  | | | | | _____  *
                        *     / /___| | | | | | _____  *
                        *  __/  ____  | | | | |______  * 
                        * |____/    |_| |_| |________| *
                        *                              *
                        *         SYSTEMS, INC.        *
                        ********************************
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2