Hello,Yap Chow Lan
The plating problem might have been caused by a very
thin layer of coverlayer residues that covered the
copper pads to be plated. After developing, the residue
layer can be too thin to be found by visual
inspection. Usually a plasma cleaning is needed to
remove it. I hope this will help.
suixin zhang
ELIS-TFCG/IMEC, University of Ghent
Sint-Pietersnieuwstraat 41, B-9000 Ghent, Belgium
tel: 0032-9-2643371
fax: 0032-9-2643594
Email: [log in to unmask]
http://www.elis.rug.ac.be/ELISgroups/tfcg/staff/sz.html

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2