WE have a situation where some electroless nickel plated items
that
come in from a vendor are some times solderable with RMA flux and
other times requires an organic acid flux to do the job.
Someone told us that the phosphorus content may make the
difference
and someone else suggested that included organics may cause this.
Any
comments or experiences with this.
################################################################