Polyclad (Cookson) is getting the licensing from GE to make Getek, but it
isn't on line yet. Until they start making what was Getek, I don't think
Polyclad had a PPO/epoxy resin system.
They do (or did?) have a PPE (like former Nelco 6000-21) resin. I believe
that was LD-621. Don't know if it's available still.
Tim Reeves
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of McGlaughlin, Jeffrey
A
Sent: Wednesday, February 25, 2004 8:47 AM
Subject: Re: IPC-4101 Material
The generic reference is to PPO (polyphenylene oxide) Epoxy/Glass
laminate. There are several manufacturers making this type of laminate,
Polyclad and Matsushita are two that come to mind. My doc's on these
materials show Er as [log in to unmask] The curve for frequency is fairly
flat from what I remember
With a high of around 3.8-4.6 at 10GHz.
By the way GeTek is no longer GeTek, GE sold the division off and was
closing the manufacturing plant where it was made. I can't remember who
bought the rights to manufacture the materials.
Hope this helps,
Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle Memorial Institute
Columbus Ohio
http://www.battelle.org
[log in to unmask]
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, February 25, 2004 10:42 AM
To: [log in to unmask]
Subject: [TN] IPC-4101 Material
Good day...
Our designers want to use an FR-4 material which is designated as
IPC-4101/25. The /25 material has a permittivity of 4.4, while the
other FR-4 materials (/21and /24) are listed as 5.4. I found out that
GETEK is classified as /25, and was wondering if this is the only /25
material available. Is there a generic (or product) name for the /25
material? The slash sheets in 4101 have a maximum permittivity at 1
Mhz, do the graphs exist that show the Dk at various frequencies?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]> 631-595-5879
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|