If Sn-Pb eutectic paste is used with a BGA with SAC balls, it is commonly
recommended to make sure that the reflow profile fully melts the SAC ball to
minimize risk of voids at the former interface of the paste and the ball.
The Xilinx temp is typical.
Best regards,
Leo
Leo M. Higgins III, Ph.D.
Director of Applications Engineering
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704
ph 512-383-4593
fx 512-383-1590
[log in to unmask]
www.asat.com
The information contained in this electronic message is CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited. If
you have received this communication in error, please immediately notify the
sender by electronic mail. Thank you.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Thursday, June 16, 2005 11:19 AM
To: [log in to unmask]
Subject: Re: [TN] WAS NTC, now BGA reballing...
Oh, if you are going that high. I must have missed that. Yes, then
voiding is going to be there, since the balls will have gone molten and
you will be using a paste flux engineered for lower temperatures.
Bev
RIM
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: June 16, 2005 11:43 AM
To: Bev Christian
Cc: TechNet E-Mail Forum
Subject: RE: [TN] WAS NTC, now BGA reballing...
Hi Bev!
According to what Xilinx says their lead-free alloy for their BGA
spheres
is SnAgCu, and liquidous is 217 C. and they want you to peak at 230 -
235
C.
for good wetting according to their reflow guidelines.
So to me, if I don't hit the recommended peak, there would be a good
chance
of voids, or am I wrong about this?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+---------------------------->
| | "Bev Christian" |
| | <[log in to unmask]
| | om> |
| | |
| | 06/16/2005 09:36 |
| | AM |
| | |
|---------+---------------------------->
>-----------------------------------------------------------------------
---------------------------------------|
|
|
| To: "TechNet E-Mail Forum" <[log in to unmask]>,
<[log in to unmask]> |
| cc:
|
| Subject: RE: [TN] WAS NTC, now BGA reballing...
|
>-----------------------------------------------------------------------
---------------------------------------|
Steve,
I am a bit confused. If you are going to use a leaded paste at say
215-220C, then you are not going to melt lead free BGA balls, so why the
concern about voiding? There is more of an issue with leaded balls in a
lead free process. Or did I miss an e-mail or two... or am I missing a
few crucial brain cells this morning? :)
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: June 16, 2005 9:55 AM
To: [log in to unmask]
Subject: Re: [TN] WAS NTC, now BGA reballing...
Mornin' Ioan!
You know, that hasn't occured to me. Maybe somebody else that
knows more about metallurgy than I do could answer. I wouldn't think
that would be a huge issue though...I might be wrong.
The point in reballing with 63/37 spheres is to avoid all the voiding
issues with lead free spheres, and to replace them with a alloy that's
better understood as far as performance and reliability is concerned.
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+---------------------------->
| | "Tempea, Ioan" |
| | <itempea@POSITRON|
| | .QC.CA> |
| | Sent by: TechNet |
| | <[log in to unmask]>|
| | |
| | |
| | 06/16/2005 07:45 |
| | AM |
| | Please respond to|
| | TechNet E-Mail |
| | Forum; Please |
| | respond to |
| | "Tempea, Ioan" |
| | |
|---------+---------------------------->
>-----------------------------------------------------------------------
---------------------------------------|
|
|
| To: [log in to unmask]
|
| cc:
|
| Subject: Re: [TN] NTC-Really, really pretty solder...
|
>-----------------------------------------------------------------------
---------------------------------------|
Hi Stevie Roy,
you might want to keep it NTC, but I see a very technical issue here.
This
is the re-balling with 63/37. The original balls were lead-free,
therefore
having created some specific intermetallics between the chip and the
ball.
If you put the leaded balls on, how reliable will be the new
intermetallics
that are formed?
Just a thought.
Regards,
Ioan
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stephen Roy Gregory
> Sent: Wednesday, June 15, 2005 11:02 PM
> To: [log in to unmask]
> Subject: [TN] NTC-Really, really pretty solder...
>
> Hi everyone!
>
> First, I want to express why I posted what I did earlier. I see all
this
> "Lead-free" stuff in
> every trade magazine that I pick-up, I get spam email from everywhere
that
> you can imagine, about lead-free seminars, training classes, why I
need
to buy
> different equipment, yada-yada-yada.
>
> But then I hear off-the-record from engineers at companies who are our
> customers, that they aren't even thinking about lead-free solders.
>
> I'm starting to look at tinning all components with standard 63/37
solder,
> re-balling BGA's with 63/37 spheres, and every other means available
to
meet our
> customer demand to stay away from anything and everything lead-free,
and
to
> try and remain competitive. On top of all of this, I will probably
have
to
> figure out how to run a lead-free line and keep everything under
control
at the
> same time, because we do have customers that will be marketing their
stuff in
> Europe... talk about alligators!
>
> We don't have a big engineering staff, or a nice lab to do experiments
or
> analysis. We're not unlike a lot of EMS companies our size. We're a
high
mix, low
> volume shop that specialize in defense and military electronics,
that's
our
> heritage. We do things in the way that has been proven, and known to
be
> reliable. When this lead-free deal was put on the table, it has turned
things upside
> down for me at least. I guess I was just trying to find out if anyone
else
> felt as p*ssed off as I am and as overwhelmed about lead-free as I do.
>
> On a lighter note, but in the same vein though, I took a cue from an
earlier
> post, and have created an image on my web page of what Tin/lead solder
might
> appear as in the year 2010.
>
> Take a look at: http://www.stevezeva.homestead.com , go to Picture
Page
2,
> and look at; "REAL Pretty Solder".
>
> -Steve Gregory-
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public
information. Any use of this information by anyone other than the
intended
recipient is prohibited. If you have received this transmission in
error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|