Leland

We have been successful cleaning the OSP with a hundred percent recovery using EnviroSense EnviroGold 816 saponifier.  If you only have 30 I would be happy to clean them at no cost thru our Aquastorm 200 if you would like to.



Terry Munson

765-457-8095

Foresite

Sent from my Verizon Wireless BlackBerry



-----Original Message-----

From:         Leland Woodall <[log in to unmask]>



Date:         Fri, 2 May 2008 15:33:40 

To:[log in to unmask]

Subject: [TN] Cleaning of OSP Oxidation





Folks,



I have about 30 OSP boards that have been processed on the bottom side,

were stashed away or misplaced for 6 to 9 months, and recently brought

to me for permission to process on the top side.



Most of these appear to have varying degrees of oxidation, as the

original light orange copper appearance has begun to look more like a 5

year old penny.



Is there a way to salvage this product?



Not only will they get the more complex components (appx. 70% of

assembly cost) during top side build, but they must also undergo wave

soldering of a 132 pin connector and several through-hole power

transistors.



I feel quite uncomfortable with doing anything other than trashing the

product...



Thanks,



Leland Woodall



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2