Dear Francis ,
There are few possibilities which could hlep you narrow down the
problem :-
1.Check your palladium bath concentration .
2.Check the electroless copper bath air agitation
3.Check the electroless copper bath auto dosing of formaldehye , caustic
and copper rate .Do set up a calibration on a weekly basis the dosing
rate and also a daily weight gain control .With the irregular dosage
of formaldhedye and high air agitation , chances of this happening is
high .However , do not overlook at the digital copper level indicator
as it may also sometimes be faulty .(If you have a unit)
Hope the above could assist you in your troubleshooting .
HH
>Have you checked the plating rate , it sounds as if the electroless copper
>bath is over active causing nodular copper growth
>I am assuming you are using high build, which Macdermid electroless is it ?
>(I am ex Macdermid Technical Sales in UK)
>
>----- Original Message -----
>From: Francis Lai <[log in to unmask]>
>To: <[log in to unmask]>
>Sent: 05 June 1999 01:56
>Subject: [TN] PTH Problem
>
>
>> We use the Macdermid PTH line. Recently, after PTH there are fluffy,
>> small minute copper deposits around the drilled holes besides the
>> electroless copper on the PTH walls. The copper surface of the panel
>> looked porous. After copper plating, they became pits on the surface of
>> the panel and nodules on the PTH walls.
>> Can any one help?
>> My e-mail : [log in to unmask]
>> THANKS!!!!!!!
>>
>> Francis
>>
>> ################################################################
>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>> ################################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in the body:
>> To subscribe: SUBSCRIBE TechNet <your full name>
>> To unsubscribe: SIGNOFF TechNet
>> ################################################################
>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>section for additional information.
>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>> ################################################################
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|