TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Peter Swanson <[log in to unmask]>
Reply To:
Date:
Fri, 3 Mar 2000 12:53:32 GMT
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
In message  <2106F62FC079D211BF2A00A0C9AA8ABF0177EFC9@SRVEXCHG> [log in to unmask] writes:
> Gabi,
>
> some time last year, I asked the same question. The result was that one of
> the prominent members of this brain assembly faxed me one paper that he
> wrote following extensive experiences. I take all the blame for forgetting
> the name and having lost the paper (actually I forwarded it to the guy that
> was taking care of this activity).
> Maybe the gentleman is still on-line and hears you.
>
> Anyway, the bottom line of the article was that the UV curable substances
> are the best. You can buy some from Dymax, along with the curing stuff.
>
> Of course, that will not help you much with the human problems, everybody
> will think they will soon get blind.
>
> Hope this helps,
> Ioan
>
> > -----Original Message-----
> > From: Bogdan Gabi [SMTP:[log in to unmask]]
> > Sent: Monday, February 28, 2000 11:35 AM
> > To:   [log in to unmask]
> > Subject:      [TN] Wire staking
> >
> > Dear TechNetters!
> > Please help with safety regulations and materials for jumper wire staking.
> > We encounter the following problems with our current cyanoacrylate:
> > - workers complain about vapor inhalation although they work with exhaust
> > units;
> > - the strength of the adhesive is very low after wave soldering - we glue
> > the jumpers before wave soldering , on C.S.
> > - please reccommend materials used successfully and which method is the
> > least harmful.
> > Thank you,
> > Gaby

Might have been me! I did write an article about this once, would be willing to
fax it. (Mental note: must put it up on the web page for the future...)

Peter
--
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
Peter Swanson                                              Oxfordshire, England
INTERTRONICS
[log in to unmask]                  http://www.intertronics.co.uk

Suppliers of materials and consumables to the electronics & related industries
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2