Yes, they do impose special design considerations. A good place to start is
IPC-7095. Which is about to rev to 7095A. There are of course many text
books on the subject. John Lau has written several.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Crain, Peter (GE
Energy)
Sent: Wednesday, September 22, 2004 12:06 PM
To: [log in to unmask]
Subject: [TN] More simple BGA questions
First: Thanks to everyone who gave feedback on my oven question......very
helpful!!
More BGA questions: Do BGAs require any special treatment when designing
PCBs? Can there be top layer traces, vias, and components near the BGA? Is
there a good general spacing around them to allow for inspection / repair?
Can BGAs be mixed with through-hole and sustain the Wave Solder process
(top-side of course) without the use of solder pallets?
Thanks again in advance,
Peter Crain, C.E.T
Manufacturing Engineering
> Network Reliability Services
> General Electric Canada Inc.
> 2728 Hopewell Place N.E., Calgary, Alberta T1Y 7J7 CANADA
> Tel: 403.214.4560, Dialcomm: 8.498.4560 Fax: 403.214.4776
> Email: [log in to unmask]
> Website: www.gepower.com/substationautomation
>
> NOTICE: The information contained in this e-mail is privileged,
> confidential and intended solely for the use of the addressee named above.
> If the reader of this e-mail is not the intended recipient, you are hereby
> notified that any dissemination, distribution or copying of this e-mail is
> strictly prohibited. If you have received this e-mail in error, please
> notify me immediately by telephone (collect) at (1) 403.214.4400 and
> destroy this e-mail as well as any copy. Thank you.
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|