TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Eric Yakobson <[log in to unmask]>
Date:
Sat, 31 Oct 1998 20:04:48 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Eric Yakobson <[log in to unmask]>
Parts/Attachments:
text/plain (147 lines)
Michael,

With all due respect, I'm afraid I have to disagree with your explanation.
While it is true that cathode current efficiency for a typical acid copper
electrolyte is close to 100%, this is exactly the reason why it does not
have any effect on current distribution.  The key to the explanation of
this phenomenon is cathode polarization (sorry for the electrochemical
terminology, but it would be rather difficult to explain this without using
it).

At low average current density the difference between cathode polarization
on lower/higher current density points of the cathode in most electrolytes
(including acid copper) is normally much greater than at high average
current density.  Therefore, the current distribution is more uniform at
low average current density.

In most alkaline electrolytes, where current efficiency is much lower than
100% (the rest of the current is consumed for hydrogen gas evolution), it
does affect the current distribution favorably.  Since at higher densities
more current is consumed for hydrogen evolution, the metal distribution
generally is more uniform then in acid solutions.

Low current density will result in higher throwing power in both systems.
One of the few practical exceptions to this rule (low current density/high
throwing power) is hex-chromium electrolyte, in which current efficiency is
directly proportional to current density.

As to the minimum copper thickness, historically (by trial & error I guess)
it was determined that 1 mil (25 micron) of copper is a minimum thickness
that will reliably withstand multiple solder floats.  From my practical
experience, 0.5 mil cracks much more readily, which is understandable,
considering the fact that copper tensile strength is proportional to the
thickness of the deposit.

Best regards.

Eric Yakobson
Alpha PC Fab






mcarano <[log in to unmask]> on 10/31/98 07:30:36 AM

To:   [log in to unmask]
cc:    (bcc: Eric Yakobson/AlphaPCFabUS/Cookson)
Subject:  Re: [TN] Copper plating & Copper thickness




Dear Francis,

The best explanation for any type of electroplating in an acid medium has
to
do with plating efficiency. Generally, acid plating process like the acid
copper, acid tin etc are close to 100% efficient. In other words, the
plating favors the high current dednsity areas of a pwb(the surface as
opposed to the hole) By lowering the cathode current density, you now tend
to favor the low current areas somewhat, and thus improve throwing power.
This works just the opposite with alkaline based plating solutions.

With respect to high frequency and plating unformity, I am not sure.
Generally, the more thickness inside the hole, the better the hole wall
plating is able to stand up to thermal excursions.

Hope this helps.

-----Original Message-----
From: Francis Lai <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Saturday, October 31, 1998 9:30 AM
Subject: [TN] Copper plating & Copper thickness


>Dear Sir :
>
>I work inn a high frequency PCB manufacturing company and I have the
>
>following questionns :
>
>1/ Why is it for copper plating (acid copper plating) the lower the
>   current, the more the throwing power ? If I start to plate copper
>   on the PTH walls with high current density after PTH, what will
>   happen ?
>
>2/ Our customer always specify to have a certainn thickness innside the
>   PTH walls for copper. Why is that so for high frequency PCB ?
>   What happen if copper thickness is thinner than the specified
>   thickness at high frequencies ?
>
>Thanks for your help !!!!!!!
>
>my e-mail : [log in to unmask](this is only text base, pls do not
send
>                                      graphics)
>
>Thamks again!!!!!!!
>
>Francis
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2