Ramon,
I never tried it, but I was told that you could heat the conductive adhesive in much the same way as with solder, and then remove the component. I can under stand how this works with small chip components, but I am not sure how this would work for large mulileaded devices unless you had hot air rework equipment for this purpose. As far as THT goes, I am not sure how you would do this. It would be best to talk to the material vendor about rework procedures.
John G
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Tuesday, November 09, 2004 8:24 AM
To: [log in to unmask]
Subject: Re: [TN] Conductive Adhesive
Anybody:
How do you remove the conductive adhesives to replace a component? Do they work for SMT as well as for THT?
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of James TerVeen
Sent: Monday, November 08, 2004 3:38 PM
To: [log in to unmask]
Subject: Re: [TN] Conductive Adhesive
I think you need to check with the conductive adhesive manufacturer.... I
my mind is still clear there were a number of them that would not work well
with tin or tin/lead plating on the parts. Most of the time these
adhesives are used with gold or silver termed parts. If you add either tin
or lead into the mix it creates a problem for reliability. But as I said
check with the conductive adhesive manufacturers. If this really worked,
you would bet that every board you would buy would be done with it and
eliminate the need for the cleaning of flux. So be very careful when you
select this to replace soldering parts to board.
John Guy
<[log in to unmask] To: [log in to unmask]
COM> cc:
Sent by: TechNet Subject: Re: [TN] Conductive Adhesive
<[log in to unmask]>
11/08/04 03:28 PM
Please respond to
TechNet E-Mail
Forum; Please
respond to John
Guy
Peter,
I a previous life I did several evaluations of conductive adhesives
as a solder replacement. You will find that the adhesive should print as
well as solder paste if you double the print speed. Other than for that,
it prints the same. I need to qualify it be saying that I did not print
fine pitch components, but I don't think this should prove to be a problem.
If you want to talk about any other results, I have a few horror stories
that I can share.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter L
Sent: Friday, November 05, 2004 8:20 PM
To: [log in to unmask]
Subject: [TN] Conductive Adhesive
Hello Technet,
Can someone share their experience on Pros/cons (in particularly process
implication) of applying conductive adhesive Vs solder paste? We have a
request by one customer to investigate conductive adhesive (stencil print
compatible) as a potential substitute for Pb-Sn solder and eventually lead-
free.
Rgds,
Peter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
STATEMENT OF CONFIDENTIALITY:
If you have received this e-mail in error, please immediately notify the
sender by e-mail at the address shown. This e-mail and any attachments may
contain confidential information. This information is intended only for the
use of the individual(s) or entity to whom it is intended even if addressed
incorrectly. Please delete it from your files if you are not the intended
recipient. Thank you for your compliance.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|