TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Fri, 10 Jan 2003 09:17:16 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mel Parrish <[log in to unmask]>
Subject:
From:
Mel Parrish <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
Hello Peter,
There was an attempt some years back to intentionally create large solder
connection as a compensation for solder joint reliability issues.  The
result was the components were overcome by the mass of the solder connection
and CTE? and was not successful but possibly enlightening here.  I think the
term used was "Bulbous Solder Connections" so you might find some
information under that term.

Mel Parrish

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of
[log in to unmask]
Sent: Thursday, January 09, 2003 6:30 PM
To: [log in to unmask]
Subject: Re: [TN] Help anyone!!!


"Drawbridging" is a new(ish) term to me, and I reasoned that if
'Tombstoning' means a component standing on end (or tending in that
direction) and 'Billboarding' means components standing on their side,
'Drawbridging', if different from the other two, would nicely describe a
phenomenon I experienced a couple of times. Depends on your design of
drawbridge, however. In my mind, I had a picture of two halves of a bridge
rising from the middle, pivoting at either end.

The phenomenon I experienced was when a couple of chip resistors sustained
damage in a strange way - the end caps and their solder joints were present
on the board, but the main body of the thing had disappeared. My initial
thoughts were impact damage, but then one affected component was right in
the midst of a veritable metropolis of discrete components, while the other
was in a completely different area of the board. I noticed that the solder
volume in the joints for these was somewhat on the high side, and concluded
that while cooling, the contraction had been enough to pull the end caps
away from the component body enough for the body itself to fall out - i.e.
it seemed that both ends had tried to tombstone at the same time, resulting
in a failure in the middle.

If anyone can refute this deduction, I would be only to pleased to hear.

Peter



Werner Engelmaier <[log in to unmask]>    10/01/2003 12:40 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to Engelmaier

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: Re: [TN] Help anyone!!!








Hi Steve,
In a message dated 01/08/2003 22:33:54, [log in to unmask] writes:
>First off, are these really "tombstones" or are they "drawbridges"? I
It has been my understanding for some 20 years that "tombstones" and
"drawbridges" are just different words for the same problem--has
soomethinng
changed?

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------




[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2