Randy,

IPC-MF-150 is the applicable standard for copper foil, however, we can 
give you a simple rule that many of the major board fabricators follow, 
unless otherwise specified, use HTE copper for all multilayer designs 
over four layers. 

Sincerely, Dan Brandler, Technical Director, Ohmega Technologies, Inc.
Http://www.ohmega.com.
 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2