TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 29 May 2007 18:09:12 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
Hi Inge,
Unfortunately, for solder joints the MTBF-concept makes little sense because 
they fail as the result of wear-out.
If you look at the wear-out of solder joints of a large population, you see 
almost a 2-order of magnitude between first failure and last failures, since 
the Weibull shape factor is about 3.
For some laptops rhyming as the one previously mentioned, out-of-the-box 
failures have been reported with most failure having occurred in ghe 12 to 24 
months range--depending on usage, of course.
The problem is a design issue with large component, large delta-CTE, large 
on/off T-difference, little lead compliancy—a textbook case of how not to do it.



Werner



**************************************
 See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2