TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Fri, 23 Mar 2001 08:57:46 -0600
Content-Type:
multipart/mixed; boundary="=_EAB16667.4524488E"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (471 bytes) , TEXT.htm (955 bytes)
I would go find out why the nickel is propsed to be eliminated.  You may find that there is a problem with the plating of the nickel with the supplier and it was someones bright idea to just eliminate the nickel ( no problem anymore) without completely thinking through what the ramifications will be further into the process.  

I feel that the nickel plating is one of the preferred methods for a flex to connect to the stainless part.  

My $.02 anyway.  
 
Kathy



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD> <BODY style="FONT: 8pt Arial; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV><FONT size=1>I would go find out why the nickel is propsed to be eliminated.&nbsp; You may find that there is a problem with the plating of the nickel with the supplier and it was someones bright idea to just eliminate the nickel ( no problem anymore) without completely thinking through what the ramifications will be further into the process.&nbsp; </FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT size=1>I feel that the nickel plating is one of the preferred methods for a flex to connect to the stainless part.&nbsp; </FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT size=1>My $.02 anyway.&nbsp;&nbsp;</FONT></DIV> <DIV><FONT size=1>&nbsp;</FONT></DIV> <DIV><FONT size=1>Kathy</FONT></DIV></BODY></HTML>