TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Temkin, Gregg" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Temkin, Gregg
Date:
Tue, 10 Mar 2009 08:09:48 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
I've had a similar experience in the past with a Kester Acid flux and they recommended a neutralizing dip with their neutralizing solution, Kester 5760, followed by a good DI rinse.  But I don't think this could help wire connections.

If this happened once, it will happen again.  Suggest finding another way to enhance flow from your selective solder nozzle.

Gregg


-----Original Message-----
From: Jim West [mailto:[log in to unmask]] 
Sent: Monday, March 09, 2009 4:45 PM
To: [log in to unmask]
Subject: [TN] Wrong flux used

During selective soldering, our operator used an IA flux (superior flux
75), which we normally use to dress up the soldering nozzle to create a
smooth flow of solder.  The flux was applied by a spray fluxer.  The
operator used the wrong bottle when reloading the spray fluxer.

We ran the boards through a wash system hoping to remove the IA flux. 

The soldering operation involves discrete wires and I would think that the
flux would wick up under the wire insulation and not be reachable for
cleaning.  
  
My questions are:

If the flux has wicked up under the wire insulator and can not be reached by cleaning, will this type of flux 
cause issues with the copper wire?

Will cleaning the boards be enough to say that no harm will be done, or
will this flux cause latent issues due to it's aggressiveness? (other
components were touched by this flux, i.e. SMT ceramic capacitors,
resistors)


Flux information 
Superior soft soldering flux:
"The inorganic acid (IA) zinc chloride fluxes, commonly referred to as
"acid fluxes," are used for industrial soft soldering applications with
tin/lead, tin/silver, and other solder combinations. These fluxes typically
contain a combination of zinc chloride, hydrochloric acid, and ammonium
chloride and are used for soldering stainless steels, brass, copper, and
other metals."

Thanks,
Jim

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2