TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Raymond Klein <[log in to unmask]>
Date:
Wed, 28 Apr 1999 16:57:52 -0700
Content-Type:
text/plain; charset="us-ascii"
X-To:
"[log in to unmask]"@gemini.adnc.com
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Raymond Klein <[log in to unmask]>
Parts/Attachments:
text/plain (18 lines)
What about good old fish paper underneath the transformer? It has high
resistance to having holes poked through it by sharp edges. On the down
side, it's flammable.

Ray Klein

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2