TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Wed, 14 Oct 1998 16:03:28 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (31 lines)
Keep in mind the IST is destructive and can only be
performed on test coupons - not actual boards.

It is not like a bare board continuity check.

You would have to do a lot of upfront design work to
make certain that your coupons could be used in the
tester.

While there has been some correlation testing performed with
thermal cycling/thermal shock type tests, the IPC is trying
to do a round robin to correlate with thermal stress testing.
However it is not going too well.


Susan Mansilla
Technical Director
Robisan Lab

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2