TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Date:
Tue, 27 Apr 2004 14:17:18 -0400
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (91 lines)
Hi Steve,

just to check, wasn't there any reversed polarity tantalum or electrolythic
at the place of the smoking hole 1?

Regards,
Ioan

> -----Original Message-----
> From: Steve Gregory [SMTP:[log in to unmask]]
> Sent: Tuesday, April 27, 2004 2:08 PM
> To:   [log in to unmask]
> Subject:      [TN] Interesting Occurance...
>
> Hi All!
>
> Just had an interesting occurance that I thought I'd share with you. We
> build
> this 14-layer assembly here that has 10 Altera FLEX 240-pin QFP's on
> it...4
> on one side, 6 on the other. We've been building this assembly for some
> time
> now with no problems.
>
> After SMT, the board goes through AOI, gets some connectors hand soldered
> on,
> then goes to ICT. After ICT it goes into a Thermotron for some power-on
> thermal cycling for eight hours.
>
> Last week, after a cycle was done, the test technician went to retrieve
> the
> boards from the oven. Upon opening the oven door, he noticed this funky
> smell....kinda like burnt fiber glass. At one of the twelve positions in
> the test
> rack he found this:
>
> Go to http://www.stevezeva.homestead.com and look at "Smoking Hole" and
> "Smoking Hole 2" (NOTE: DUE TO THE GRAPHIC NATURE OF THESE IMAGES,
> PARENTAL
> DISCRETION IS ADVISED)
>
> We don't have a clue how this happened. ICT on this assembly was fine,
> there
> were no problems found in the test fixture position in the oven (other
> assemblies have gone through the temp cycle in the same position without a
> problem).
> And supposedly, there is only 5V and 3.3V being applied during the thermal
> cycle.
>
> Obviously there had to be more voltage than that to cause the kind of
> damage
> you see in the pictures, but nobody knows where it came from. Smoking Hole
> is
> a QFP on one side of the board, and Smoking Hole 2 is on the other. The
> leads
> are vaporized in the pictures. This only happened to one board, and the
> fixture was loaded up with another 11-assemblies.
>
> I don't expect we'll ever figure out what happened unless it somehow
> happens
> again. I know one thing, if it does, I don't want to be anywhere near the
> oven!
>
> Thought you might find the pictures interesting...these are $4000 images.
>
> -Steve Gregory-
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2