TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 15 Jun 2005 08:06:51 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (220 lines)
Steve,

More technical people have to ask questions when there isn't data to support a direction. I for one don't want to be one of those people that as you said (Let's all of us jump off the cliff, and say in the end; "We did what
we were supposed to...".  The majority of career was spent under the Ma-Bell umbrella and I enjoyed being associated with Bell Laboratories where decisions used to be made for sound technical reasons and always supported by data.  It is disheartening to see supply chain, bottom line economics, and bureaucracy making the decision without having supporting data.  I wouldn't have take Bev's comment personal and if I were Bev I wouldn't apologize for making them.  Those kinds of comments are made by all of us who's working world has been turned upside down trying to deal with Pb-Free issues.

Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen Gregory
Sent: Wednesday, June 15, 2005 7:42 AM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why? NTC


Bev,

I never have considered people on this distinguished list "my personal
entertainment".
I'm sorry that you think that, and apologize sincerely if I have come
across that way.

As I said, it was the first time I have ever read that article, and I
thought that it's very
detailed and lucid about this whole lead-free thing.

Call me naive (which I probably am), I just don't understand why our
industry is being
turned upside down like this...maybe I don't know how things work.

I'm sorry I've wasted your time. Please forgive me.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX



                      "Bev Christian"
                      <[log in to unmask]        To:       "TechNet E-Mail Forum" <[log in to unmask]>, <[log in to unmask]>
                      om>                      cc:
                                               Subject:  RE: [TN] Lead-Free, Why? NTC
                      06/15/2005 06:28
                      AM






I will be REAL blunt.  Come on. Steve.  You have been around long enough
to know how things work.  We are not here for your personal
entertainment, we have jobs to do.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: June 14, 2005 10:17 PM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free, Why?

I was kind of suprised that there was only one private response
to my post about this...I guess we all are sheep.

Let's all of us jump off the cliff, and say in the end; "We did what
we were supposed to..."

Then live with it all...

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX




                      Stephen R Gregory
                      (Tulsa)                  To:       [log in to unmask]
                                               cc:
                      06/14/2005 08:38         Subject:  [TN] Lead-Free,
Why?
                      AM





Mornin' Everyone!

Yesterday I had one of our test technicians come to me and
ask if I knew of any good reference articles about the pro's and
cons of Lead-free solders.

He's doing a assignment in his college class about manufacturing
processes. I first went on my rant about how mis-guided this whole
thing is, and then told him that I was sure I could find him some good
references.

I did a search and found one that I had never seen before, and after
reading it, I think it's the best one I've read. Go to:

http://www.cepelec.com/iso_album/leadfreehmiller.pdf

It's 53-pages, and very, very good!

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.


__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2