Dear Mr. Engelmaier,
Thanks for your reply. The PBGA under modeling is 1.0mm pitch, 25-mil
balls. ATC is 0-100C, 2 cycles/hr. In one case study, the package size is
27x27mm, die size 21x21mm, die thickness is 12mil, full array with ball
count of 672. The predicted CMF when using 15-mil and 24-mil thick BT
substrate is 839 and 6653 cycles respectively. The adopted approach is
substructure and micro-model approach. First, the whole package
was meshed and treated as a substructure except the solder joint of
interest (under the corner of die); then a substructure analysis was done
to generate stiffness matrix; In micro model, the solder joint of interest
was modeled in detail and creep analysis was done. I use ANSYS 5.4.
Please let me know if you need more information.
Regards,
Yuan Li
On Sat, 29 May 1999, Werner Engelmaier wrote:
> Hi Yuan,
> This increase is possible only if the thickness increase substantially
> reduces the warpage of the PBGA or substantially decouples the influence of
> the die on the global expansion mismatch. It still sounds too large, though.
> To say something more, I need the full details of your analysis and some of
> the result details.
>
> Werner Engelmaier
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|