I'm sure you know this, but checking flux specific gravity (in accordance with supplier requirements
at a specified temperature) with a calibrated hygrometer is best. Worst, is using so called
automatic systems that are part of some wave solder machines. Also, don't keep replenishing or
"thinning" flux. It's cheap, compared to defective solder joints, so dump and replace regularly
(when sg starts falling off say at the end of a shift or production run). Hope I didn't over-
simplify, but it's all I know.
Earl Moon
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|